Videos / Silica sand demo

Silica Sand Iron Removal — PTMS Magnetic Separator Demo (Saudi Arabia)

Real workshop footage of a PTMS electromagnetic separator treating silica sand from Saudi Arabia. Segment order: raw sand → feed in / clean product out below → iron captured by the magnetic matrix. No after-separation figures are published here — your own sample decides the result.

Related: Silica sand production line · All videos · Silica sand iron removal guide (powtechina.com) · Dry separator for quartz: buyer guide (ptmsmagnet.com)

Silica Sand Iron Removal — PTMS Magnetic Separator Demo (Saudi Arabia) 1:30 — How to remove iron from silica sand: factory demo of a silica sand magnetic separator on sand from Saudi Arabia: raw sand is fed into a PTMS electromagnetic separator; clean product discharges below, and iron is captured on the magnetic matrix. No performance numbers claimed — your own sample decides the result.

After magnetic iron removal

Product look after two passes on the PTMS magnetic separator. Lab assay for this product will be published separately when available — no product numbers are shown here.

Silica sand after two passes of magnetic iron removal (Saudi Arabia)
Silica sand after two passes of magnetic iron removal (Saudi Arabia)

Feed material: raw silica sand analysis (Saudi Arabia, Oct 2026)

The table below is the raw feed before magnetic separation — the same type of silica sand shown in the video. Figures are as reported for this feed lot (%). This page does not publish after-separation results.

Separation results vary by ore and are confirmed by a pilot test. Send 5–10 kg of your material; we deliver a test report within 5 days of receiving the sample.

Particle size distribution (result %)

SieveResult %
#200
#250
#351.14
#14095.42
Pan3.44

Chemical composition (result %)

ItemResult %
SiO₂98.806
Al₂O₃0.396
Fe₂O₃0.013
Na₂O0.359
TiO₂0.089
CaO0.317
ZrO₂0.001
Cr₂O₃0
K₂O0.009
Moisture0.12
LOI0.01
Bulk density1.04

Register for your free ore test — then a line proposal

The free ore test is for registered members. Register (free, verified on WhatsApp), then send 5–10 kg of your material — every ore is different — and we test it free with a report within 5 days of receiving the sample. Price on request.

Dry-powder separation: selection and test conditions

This footage illustrates the material and equipment described on this video page. Unless explicitly documented, it does not establish a particular machine model or quantitative separation performance. Application footage and magnetic-rod checks are not substitutes for a laboratory report or chemical analysis.

Dry powder and slurry require different process arrangements. Select the equipment from material state, particle-size distribution, moisture, flowability, bulk density, feed stability and the nature of the iron or magnetic foreign matter. A representative-sample test confirms the appropriate configuration and operating conditions.

Model specifications are not interchangeable. Cavity size, coil power, cooling, magnetic matrix and outlet or discharge arrangements must be confirmed for the selected model. Do not transfer a similar machine’s particle-size limits, dimensions, capacity or outlet positions to another model. A design-capacity range alone does not establish the lowest operable feed rate.

State the magnetic-field measurement location and conditions. Empty-bore (air-core), working-cavity and matrix-surface fields are different measurements; do not equate them or infer one from another. A series reference is not a measured result for an individual machine.

Capturing magnetic particles is not the same as reducing chemically measured total iron. Results depend on the material and test conditions. No fixed iron-removal rate, final iron-content value or titanium reduction is promised.

Free 5–10 kg lab test; report within 5 days of receiving the sample. Results apply to the sample received and the recorded conditions; acceptance requires assessment against the agreed product requirements.